Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 27.0 MPa | 3920 psi | ASTM D790 |
Rotuba MSS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Yield Strength | 27.0 MPa @Thickness 6.40 mm |
3910 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5208 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Yield Strength | 27.0 MPa | 3920 psi | ISO 178 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Flexural Yield Strength | 27.0 - 72.0 MPa | 3920 - 10400 psi | Average value: 48.2 MPa Grade Count:22 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |