Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 26300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 96.0 - 181 MPa

@Temperature 100 - 200 °C
13900 - 26300 psi

@Temperature 212 - 392 °F
Average value: 119 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 96.0 - 181 MPa

@Strain 3.50 - 5.00 %
13900 - 26300 psi

@Strain 3.50 - 5.00 %
Average value: 119 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 68.9 - 181 MPa
10000 - 26300 psi
Average value: 104 MPa Grade Count:28
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Flexural Yield Strength 181 - 181 MPa

@Temperature 232 - 232 °C
26300 - 26300 psi

@Temperature 450 - 450 °F
Average value: 181 MPa Grade Count:1
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 96.0 - 181 MPa

@Temperature 100 - 200 °C
13900 - 26300 psi

@Temperature 212 - 392 °F
Average value: 154 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Flexural Yield Strength 96.0 - 181 MPa

@Strain 3.50 - 5.00 %
13900 - 26300 psi

@Strain 3.50 - 5.00 %
Average value: 154 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Flexural Yield Strength 13.4 - 181 MPa
1950 - 26300 psi
Average value: 47.7 MPa Grade Count:128
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Copyright © lookpolymers.com All Rights Reserved