Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM D790 |
NYCOA 27/300I Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM Data |
BASF Capron® SEG6 H1 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG6 H1 is a 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthetics at the slower fill s.. |
|||
Flexural Yield Strength | 245 MPa | 35600 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN133G33SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 245 MPa @Thickness 3.20 mm |
35600 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/10 Nylon 66, 30% GFR, 10% PTFE Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silic.. |
|||
Flexural Yield Strength | 245 MPa | 35600 psi | ASTM D790 |
Cheng Yu Plastic N6G10 Nylon 6, 10% Glass Filled |
|||
Flexural Yield Strength | 245 MPa | 35600 psi | ASTM D790 |
Cheng Yu Plastic N6GV25 Flame Retardant Nylon 6, 25% Glass Filled |