Mechanical Properties Metric English Comments
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber
PET – Flame Retardant 30% Short Glass Fiber Reinforced. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM s..
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East)
High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/..
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved.
Flexural Yield Strength 168 MPa
24400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated.