Polymer Property : Flexural Yield Strength = 242 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 242 MPa
35100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
Flexural Yield Strength 242 MPa
35100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed)
Flexural Yield Strength 242 MPa
35100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive.