Polymer Property : Flexural Yield Strength = 23000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 158.6 MPa
23000 psi
ASTM D790
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Yield Strength 159 MPa
23000 psi
Sheet Stress
Hardwire 3SX-4-12 Low Density Composite
The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as w..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES HiFill FR® PA6 GF25 FR IM 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame Retardant and Impact ModifierFeatures: Flame Retardant and Impact Modifi..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES Luriblend® PC GF20 TL10 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, In..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES Plaslube® J-50/20/TF/10 Polycarbonate, 20% GFR, 10% PTFE
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Clariant Renol PA213G15 Nylon 6, 15% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..