Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 22.8 - 37.9 MPa | 3310 - 5500 psi | Average value: 29.8 MPa Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Flexural Yield Strength | 22.8 MPa | 3310 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 22.8 MPa | 3310 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 22.8 MPa | 3300 psi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR-N Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 22.8 MPa | 3300 psi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR-N V2 Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 22.8 MPa | 3310 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 22.8 MPa | 3310 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |