Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 147 MPa | 21300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | DIN 53455; ASTM D790 |
Kolon KOPET® KP133135 FR-PET Resin
(discontinued **) KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p.. |
|||
Flexural Yield Strength | 147 MPa @Thickness 6.40 mm |
21300 psi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP2100-KA02 PC+CF Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF434HR PBT PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GX05053 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX05053 is a compound based on Polysulfone blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN® A5624 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN® B5526 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN® B6528 40% GF PBT/ABS Alloy Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN®-N ASG30 SAN resin Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN®-N GRSJ3 30% GF SAN resin Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Toyobo T-400 Nylon, 15% Glass-Reinforced Key Feature: G.F. 15%Information provided by Toyobo Co., Ltd |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Toyobo Vylopet® EMC615 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | 2 mm/min; ISO 178 |
Eurostar Starflam PX05004 PA66, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Cheng Yu Plastic FR200GV25 Flame Retardant Nylon 66, 25% Glass Fiber |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Cheng Yu Plastic FV30720 POM, 20% Mineral Reinforced |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Cheng Yu Plastic FV30G10 POM, 10% Glass Fiber |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |
|||
Flexural Yield Strength | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |