Mechanical Properties Metric English Comments
Flexural Yield Strength 21.4 MPa
3100 psi
ASTM D790
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 21.4 MPa
3100 psi
ASTM D790
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Yield Strength 21.4 MPa
3100 psi
ASTM D790
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 21.4 MPa
3100 psi
ASTM D790
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 21.4 - 65.0 MPa
3100 - 9430 psi
Average value: 37.8 MPa Grade Count:86
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..