Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 89.6 - 138 MPa | 13000 - 20000 psi | Average value: 109 MPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Yield Strength | 68.9 - 138 MPa | 10000 - 20000 psi | Average value: 106 MPa Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Yield Strength | 72.4 - 138 MPa | 10500 - 20000 psi | Average value: 103 MPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Flexural Yield Strength | 96.1 - 138 MPa | 13900 - 20000 psi | Average value: 110 MPa Grade Count:4 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Flexural Yield Strength | 90.0 - 138 MPa | 13100 - 20000 psi | Average value: 110 MPa Grade Count:8 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Flexural Yield Strength | 35.0 - 138 MPa | 5080 - 20000 psi | Average value: 110 MPa Grade Count:15 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |