Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 945A PC (Asia Pacific) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX1832 PC MFR=3.0; Branched extrusion grade for LED applications, UV stabilized; available in diffuse colors |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2571T PC Copolymer Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 955 PC (Asia Pacific) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |