Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PKN4736 PPE+PS (Asia Pacific) PPE+PS. FDA compliant. High heat. Excellent ESCR. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer |