Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 138 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 89.6 - 138 MPa
13000 - 20000 psi
Average value: 109 MPa Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 68.9 - 138 MPa
10000 - 20000 psi
Average value: 106 MPa Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Flexural Yield Strength 72.4 - 138 MPa
10500 - 20000 psi
Average value: 103 MPa Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Flexural Yield Strength 96.1 - 138 MPa
13900 - 20000 psi
Average value: 110 MPa Grade Count:4
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..
Flexural Yield Strength 90.0 - 138 MPa
13100 - 20000 psi
Average value: 110 MPa Grade Count:8
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Flexural Yield Strength 35.0 - 138 MPa
5080 - 20000 psi
Average value: 110 MPa Grade Count:15
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..