Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 1100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 1100 MPa
160000 psi
ASTM D790
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC  (discontinued **)
QC-8805 is a vinyl ester-based sheet molding compound (SMC) reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness, and fatigue resistance in the fiber ..
Copyright © lookpolymers.com All Rights Reserved