Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 72.0 - 103 MPa | 10400 - 15000 psi | Average value: 89.2 MPa Grade Count:24 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 72.0 - 86.0 MPa | 10400 - 12500 psi | Average value: 81.1 MPa Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM-D790 |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Flexural Yield Strength | 71.7 MPa | 10400 psi | ASTM D790 |
PlastxWorld CEVIAN®-V 400T ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Eastman PROVISTA Copolymer PETG Copolyester Color, b* CIELAB, Illuminant D6500, 10° Observer is 0.61 per ASTM D 2244.Product Description: PROVISTA Copolymer is a resin specifically developed for extrusion into profiles where aesthetics like.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® FS 2000 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosityAs of 1 S.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Kleerdex Kydex® 160 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated. |