Polymer Property : Film Tensile Strength at Break, TD = 70.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 70.0 MPa

@Thickness 0.0250 mm
10200 psi

@Thickness 0.000984 in
ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ASTM D882
DuPont™ Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is special..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ASTM D882
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU)
Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU ..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ISO 527-3
EMS-Grivory Grivory® CR 8 PA*
Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ISO 527-3
EMS-Grivory Grivory® L 25 G nat 6011 PA12
Product Description: Grilamid L 25 G natural 6011 is a high viscosity, lubricated polyamide 12. This product has the following features: Very tastelessHigh toughness, even at low temperaturesGood re..
Film Tensile Strength at Break, TD 70.0 MPa
10200 psi
ISO 527-3
EMS-Grivory Grivory® L 25 nat PA12
Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go..