Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 44.6 MPa | 6470 psi | Calculated from mfr's report of 119 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Film Tensile Strength at Break, TD | 44.6 MPa | 6470 psi | Calculated from mfr's report of 145 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |