Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | >= 39.3 MPa | >= 5700 psi | ASTM D 882 A |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor LT74113 Hexene Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74113 is a high strength hexene linear low density polyethylene containing no slip and medium antiblock. It is designed for blown film applications and is well suited .. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor LT74119 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor LT74147 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74147 is a high strength linear low density polyethylene containing medium slip and high antiblock. It is designed for blown film applications and is well suited for c.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | ASTM D882 |
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin .. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. .. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Film Tensile Strength at Break, TD | 39.3 MPa | 5700 psi | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |