Polymer Property : Film Tensile Strength at Break, TD = 5410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 37.3 MPa
5410 psi
ASTM D882
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Film Tensile Strength at Break, TD 37.3 MPa
5410 psi
ASTM D882
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b..