Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble.. |
|||
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 3.1 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng.. |
|||
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |