Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 36.5 MPa | 5290 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Film Tensile Strength at Break, TD | 36.5 MPa | 5290 psi | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Film Tensile Strength at Break, TD | 36.5 MPa | 5290 psi | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Film Tensile Strength at Break, TD | 36.5 MPa | 5290 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |