Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 35.2 MPa
5110 psi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol..
Film Tensile Strength at Break, TD 35.2 MPa
5110 psi
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi..
Copyright © lookpolymers.com All Rights Reserved