Polymer Property : Film Tensile Strength at Break, TD = 5000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 20.7 - 34.5 MPa
3000 - 5000 psi
ASTM D882
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell..