Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the ..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin
Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Iran Petrochemical (PCC) Arak 0410AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer
The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high ..
Film Tensile Strength at Break, TD 33.0 - 39.0 MPa
4790 - 5660 psi
Average value: 36.7 MPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film
LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film
LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film
This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip ..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
Cast Film at 1.25 mil; ASTM D-882
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
Bapolene® 350F Polyethylene, Film Grade
Applications: Blown film extrusion of T-shirt sacks, merchandise bags.Film properties below are based on a thickness of .8 mil and blow-up ratio of 4:1.Bapolene® and Bapolan® are registered tradem..
Film Tensile Strength at Break, TD >= 33.0 MPa
>= 4790 psi
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl..
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl..