Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 15 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 18 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 20 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 30 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 35 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 20 µm)
PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm)
PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm)
PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm)
PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm)
PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm)
PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm)
PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 30 µm)
PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh..
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm)
PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh..