Polymer Property : Film Tensile Strength at Break, TD = 4210 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ISO 527-3
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ISO 527-3
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring ..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
LyondellBasell Montell 16502F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
LyondellBasell Montell 16502F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
LyondellBasell Montell 16502F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
UBE 1022FDX23 Nylon 6 Homopolymer Film
Specialties: High slip typeProcessing: Water cooling processTypical applications: small pouch & generalInformation provided by UBE.
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
Calculated from mfr's report of 78 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a..
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882
Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
Film Tensile Strength at Break, TD 29.0 - 303 MPa
4210 - 44000 psi
Average value: 128 MPa Grade Count:21
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..