Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica.. |
|||
Film Tensile Strength at Break, TD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App.. |