Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
M. Holland Company LL104 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
M. Holland Company MAGMA® LM115-B LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Film Tensile Strength at Break, TD | 27.6 - 37.9 MPa | 4000 - 5500 psi | ASTM D882 |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, TD | 27.6 - 41.4 MPa | 4000 - 6000 psi | ASTM D882 |
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, TD | 27.6 - 41.4 MPa | 4000 - 6000 psi | ASTM D882 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, TD | 27.6 - 48.3 MPa | 4000 - 7000 psi | ASTM D882 |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74558 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives... |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
Dow INTEGRAL™ 936 High Heat Monolayer Adhesive Film INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fi.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | ASTM D882 |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | |
3M 901 Repulpable Forms-Splicing Tape 3M™ Repulpable Forms-Splicing Tape 901 is a semi-bleached kraft paper coated with a light green repulpable adhesive.Information provided by 3M |
|||
Film Tensile Strength at Break, TD | 27.6 MPa | 4000 psi | |
3M 9114 Butt Splicing Tape 3M™ Butt Splicing Tape 9114 is a single-coated blue repulpable splicing tape which is covered with a center slit repulpable paper liner, and additionally laminated with a single coated non-repulpab.. |