Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 269 MPa | 39000 psi | ASTM D882 |
Total PPH 3270 Polypropylene Homopolymer, High Crystallinity, Low Melt Flow Film Grade Low Residuals TOTAL Polypropylene 3270 utilizes the TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock. 3.. |
|||
Film Tensile Strength at Break, TD | 269 MPa | 39000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 834 Polyester Film, 48 Gauge Mylar® 834 is a packaging grade polyester film, chemically pretreated on one side for controlled COF and release.Approvals: FDA Food Contact Status - All gauges of Mylar® 834 comply with the Food .. |
|||
Film Tensile Strength at Break, TD | 269 MPa | 39000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge Mylar® 840 is a one-side pretreated polyester film for improved metal or cold seal adhesion. The packaging industry is constantly setting higher standards for product protection using flexible pack.. |
|||
Film Tensile Strength at Break, TD | 269 MPa | 39000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Melinex® 800 is a clear, non-pretreated base film with high gloss, low haze and excellent processability. Melinex® 800 is available in 48 gauge. Meline.. |