Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 26.5 MPa | 3840 psi | ASTM D882 |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Film Tensile Strength at Break, TD | 26.5 MPa | 3840 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d.. |
|||
Film Tensile Strength at Break, TD | 26.5 MPa | 3840 psi | ASTM D882 |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Film Tensile Strength at Break, TD | 26.5 MPa | 3840 psi | |
Kuraray HYBRAR® BF3 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Film Tensile Strength at Break, TD | 26.5 MPa | 3840 psi | Calculated from mfr's report of 35 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Film Tensile Strength at Break, TD | 26.5 - 31.8 MPa | 3840 - 4610 psi | |
3M 6146 Kraft Medium Duty Reinforced Water Activated Tape 3M™ Medium Duty Reinforced Water Activated Tape 6146 Kraft is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and high tack water activ.. |
|||
Film Tensile Strength at Break, TD | 26.5 - 40.7 MPa | 3840 - 5900 psi | Average value: 33.8 MPa Grade Count:17 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |