Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 125 BSR-ONE OPP Film Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF.. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | 20 in/min, 2.0 in Jaw Separation; 510 |
ExxonMobil Bicor® 140 BSR-ONE OPP Film Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF.. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 426 Polyester Film, 92 Gauge Melinex® 426 is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. Melinex® 426 is chemically treated on one side for static control. The tre.. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 426P Polyester Film, 92 Gauge Melinex® 426P is a slightly hazy film with excellent handling characteristics. Melinex® 426P is chemically treated on one side to minimize static charge. The treatment provides stable antistatic p.. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge Melinex® 595 is a high clarity film that is one side pretreated to provide anti-charge protection and one side pretreated to promote adhesion to many solvent coating formulations. This film is exce.. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | 50% Strain rate; ASTM D882A |
DuPont Teijin Films Melinex® 542 Polyester Film Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sidesGeneral Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 142 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Break, TD | 255 MPa | 37000 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |