Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 24.5 MPa | 3550 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin
(discontinued **) LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin.. |
|||
Film Tensile Strength at Break, TD | 24.5 MPa | 3550 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin
(discontinued **) LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Film Tensile Strength at Break, TD | 24.5 MPa | 3550 psi | 500mm/min, Ultimate; ASTM D638 |
LG Chemical SEETEC BF315 LDPE Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Film Tensile Strength at Break, TD | 24.5 MPa | 3550 psi | ASTM D882 |
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Film Tensile Strength at Break, TD | 24.5 - 38.2 MPa | 3550 - 5540 psi | Average value: 31.0 MPa Grade Count:7 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Film Tensile Strength at Break, TD | 24.5 MPa | 3550 psi | |
Kuraray HYBRAR® BF1 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w.. |