Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
Kuraray HYBRAR® CF1 Mono Layer Cast Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
ExxonMobil LL 1001x59 Blown Film Resin  (discontinued **)
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Film Tensile Strength at Break, TD 35.3 MPa
5120 psi
ASTM D882
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..