Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.2 MPa | 3220 psi | ASTM D 882 |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Film Tensile Strength at Break, TD | 22.2 MPa | 3220 psi | |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |