Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 216 MPa | 31300 psi | ASTM D882A |
DuPont Teijin Films Melinex® 238 Polyester Film Melinex® 238 is a translucent white polyester film used for electrical insulation. It has been specially developed for use as an electrical insulation material in rotating electrical machines. It i.. |
|||
Film Tensile Strength at Break, TD | 216 MPa | 31300 psi | ASTM D882A |
DuPont Teijin Films Melinex® 618 Polyester Film, 700 Gauge Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide ra.. |