Polymer Property : Film Tensile Strength at Break, TD = 3130 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 21.6 MPa
3130 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene
LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
Film Tensile Strength at Break, TD 21.6 MPa
3130 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene
LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Film Tensile Strength at Break, TD 21.6 MPa
3130 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene
LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact ..