Polymer Property : Film Tensile Strength at Break, TD = 303 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 193 - 303 MPa
28000 - 44000 psi
ASTM D882
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Film Tensile Strength at Break, TD 193 - 303 MPa
28000 - 44000 psi
ASTM D882
Honeywell Capran® Emblem™ 1200 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Film Tensile Strength at Break, TD 193 - 303 MPa
28000 - 44000 psi
ASTM D882
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh..
Film Tensile Strength at Break, TD 193 - 303 MPa
28000 - 44000 psi
ASTM D882
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Film Tensile Strength at Break, TD 29.0 - 303 MPa
4210 - 44000 psi
Average value: 128 MPa Grade Count:21
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..