Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 25 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 40 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 50 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 25 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 40 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 50 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 25 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 30 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 40 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 50 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 30 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 40 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 50 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 18 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 20 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 30 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 40 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Film Tensile Strength at Break, TD | 300 MPa | 43500 psi | ASTM-D882 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |