Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 274 MPa | 39800 psi | ASTM D882A |
DuPont Teijin Films Melinex® 693 Polyester Film Melinex® 693 is a super clear polyester film pretreated on one side to promote adhesion with improved handleability.General Product Info: Melinex® 693 is a high clarity, non-yellow base with excel.. |
|||
Film Tensile Strength at Break, TD | 274 MPa | 39800 psi | ASTM D882A |
DuPont Teijin Films Melinex® 694 Polyester Film Melinex® 694 is a super clear polyester film pretreated on two sides to promote adhesion with improved handleability.General Product Info: Melinex® 694 is a high clarity, non-yellow base with exce.. |
|||
Film Tensile Strength at Break, TD | 274 MPa | 39700 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 100 Gauge Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It i.. |