Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 18.6 - 284 MPa | 2700 - 41100 psi | Average value: 32.9 MPa Grade Count:80 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM-D882 |
Westlake EB171 MDPE Medium Density Polyethylene Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF378 Low Density Polyethylene WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.Application/UsesDiaper linersGeneral purpose cl.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF412 Low Density Polyethylene WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF421 Low Density Polyethylene WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF601 Low Density Polyethylene Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | ASTM D882 |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa | 2700 psi | |
Dow LDPE 768A Low Density Polyethylene, Film Grade DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a.. |
|||
Film Tensile Strength at Break, TD | 18.6 MPa @Thickness 0.0356 mm |
2700 psi @Thickness 0.00140 in |
ASTM D-882 |
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of .. |