Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Eastman E6838-923F Polyethylene
(discontinued **) E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1041 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ISO 527-3 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Film Tensile Strength at Break, TD | >= 18.0 MPa | >= 2610 psi | ASTM D882 |
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | 500 mm/min; ISO 527-3 |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | ASTM D882 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |
|||
Film Tensile Strength at Break, TD | 18.0 MPa | 2610 psi | 500 mm/min; ISO 527-3 |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |