Polymer Property : Film Tensile Strength at Break, TD = 255 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 255 MPa
37000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor® 125 BSR-ONE OPP Film
Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
20 in/min, 2.0 in Jaw Separation; 510
ExxonMobil Bicor® 140 BSR-ONE OPP Film
Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® 426 Polyester Film, 92 Gauge
Melinex® 426 is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. Melinex® 426 is chemically treated on one side for static control. The tre..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® 426P Polyester Film, 92 Gauge
Melinex® 426P is a slightly hazy film with excellent handling characteristics. Melinex® 426P is chemically treated on one side to minimize static charge. The treatment provides stable antistatic p..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge
Melinex® 595 is a high clarity film that is one side pretreated to provide anti-charge protection and one side pretreated to promote adhesion to many solvent coating formulations. This film is exce..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge
Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
50% Strain rate; ASTM D882A
DuPont Teijin Films Melinex® 542 Polyester Film
Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sidesGeneral Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 142 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Copyright © lookpolymers.com All Rights Reserved