Polymer Property : Film Tensile Strength at Break, TD = 248 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 248 MPa
36000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor® 70 HSH OPP Film
Product Description: Bicor HSH is a one-side treated, one-side sealable, coextruded OPP film designed for use in unsupported plain or surface print high-speed horizontal applications.Availability: ..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 314 Polyester Film, 200 Gauge
Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont.
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 314 Polyester Film, 92 Gauge
Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont.
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 142 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 200 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 300 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 400 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 500 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 700 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 453 Polyester Film, 92 Gauge
Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 200 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 400 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 500 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 700 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 92 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 455 Polyester Film
Melinex® 455 is a high clarity polyester film pretreated on one side for slip. It has excellent handling characteristics.General Product Info: Two smooth coatable surfacesLow surface resistivityCan..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 456 Polyester Film
Melinex® 456 is an excellent handling, high clarity polyester film with both sides pretreated for slip. The two smooth surfaces allow easy top coating.Approvals: UL 94 VTM-2 - for 200 - 700 gauge (..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Informati..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 92 Gauge
Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge
Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.Als..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 142 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 454 Polyester Film, 300 Gauge
Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as..
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
DuPont Teijin Films Melinex® 457 Polyester Film, 200 Gauge
Melinex® 457 is one side slip, one side adhesion promoting, super clear, polyester film for color proof applications.Also available in 650 gaugeInformation provided by DuPont.