Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
Iran Petrochemical (PCC) 16503 Linear Low Density Polyethylene 16503 is a LLDPE for general purpose cast stretch film grade. The ease of processing and the low gels make 16503 well suited for production of general purpose monolayer or multilayer cast stretch fi.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3490 psi | ASTM D882 |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3490 psi | ASTM D882 |
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3490 psi | ASTM D882 |
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ISO 527-3 |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3490 psi | ASTM D882 |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3490 psi | ASTM D882 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM-D882 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM-D882 |
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM D882 |
ExxonMobil Escorene® LD-713 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM-D882 |
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag.. |
|||
Film Tensile Strength at Break, TD | 24.0 MPa | 3480 psi | ASTM-D882 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |