Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | |
Reliance Industries LLDPE film - Inorganic salt based film Information provided by Reliance Industries |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Eastman 1840F Polyethylene
(discontinued **) Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman PE5020 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms t.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Film Tensile Strength at Break, TD | 16.0 - 47.0 MPa | 2320 - 6820 psi | Average value: 31.7 MPa Grade Count:23 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, TD | 16.0 MPa | 2320 psi | ASTM D882 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |