Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 23.5 MPa | 3410 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Film Tensile Strength at Break, TD | 23.5 MPa | 3410 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Film Tensile Strength at Break, TD | 23.5 MPa | 3410 psi | 500mm/min, Ultimate; ASTM D638 |
LG Chemical SEETEC BF410 LDPE Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG .. |
|||
Film Tensile Strength at Break, TD | 23.5 MPa | 3410 psi | 500mm/min, Ultimate; ASTM D638 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |