Polymer Property : Film Tensile Strength at Break, TD = 23.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 23.2 MPa
3370 psi
ASTM D882
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Film Tensile Strength at Break, TD 23.2 MPa
3370 psi
ASTM D882
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Film Tensile Strength at Break, TD 23.2 MPa
3370 psi
ASTM D882
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Film Tensile Strength at Break, TD 23.2 MPa
3370 psi
ASTM D882
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Film Tensile Strength at Break, TD 23.2 MPa
3360 psi
ASTM D882
ExxonMobil LD 334.57 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 23.2 MPa
3360 psi
ASTM D882
ExxonMobil LD 334.82 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Copyright © lookpolymers.com All Rights Reserved