Polymer Property : Film Tensile Strength at Break, TD = 20.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 20.6 MPa
2990 psi
ASTM D882
LG Chemical LUTENE BB0808 LDPE Blown Film Grade
Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc..