Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 131 MPa
19000 psi
ASTM D882
Dow Saran® 520 Clear Plastic Barrier Film
Saran™ 520 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 2 gauge.Information provided by Dow