Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 124 MPa | 18000 psi | ASTM D882 |
Dow SARAN WRAP™ 18 Plastic Film SARAN WRAP™ 18 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double would roll.. |
|||
Film Tensile Strength at Break, TD | 124 MPa | 18000 psi | ASTM D882 |
Dow Saran® 8 Clear Plastic Barrier Film Saran™ 8 is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double wound rolls.Information provi.. |